MIG wire for mild steels & high tensile steels (490Mpa)
Ø 0.8 mm Ball Pack
Ø 1.0 mm Ball Pack
Ø 1.2 mm Ball Pack
Classifications
AWS A5.18/ ASME SFA5.18 ER70S-6
EN ISO 14341-A G 42 2 C1 3Si1
EN ISO 14341-A G 42 4 M21 3Si1
Developed by Cactus