Cored wire for stainless steels
Ø 1.2 mm (Code, SW-309MoL Cored – Ø1.2mm)
Classifications
AWS A5.22/ ASME SFA5.22 E309LMoT1-1/-4
EN ISO 17633-A-T 23 12 2 L P M21/C1 2
• 22%Cr-12%Ni-2.5%Mo stainless steels
• Dissimilar welds between carbon, low alloy steels to stainless
steels
• Buffer layer welding for cladding, overlays
Features
• Good performance in all positions
Developed by Cactus