Stick electrodes for low temperature service steels
Ø 2.6 mm x 350 mm x 5 kg (Code, 7018.1H 2.6mm x 350mm)
Ø 3.2 mm x 350 mm x 5 kg (Code, 7018.1H 3.2mm x 350mm)
Ø 4.0 mm x 400 mm x 5 kg (Code, 7018.1H 4.0mm x 350mm)
Classifications
AWS A5.1/ ASME SFA5.1 E7018-1 H4R
EN ISO 2560-A-E42 4 B 3 2 H5
Developed by Cactus