Cored wire for stainless steels
Ø 1.6 mm x 15 kg (Code, SUPERCORED 308L1.6mm x 15kg)
Classifications
AWS A5.22/ ASME SFA5.22 E308LT0-1/-4
EN ISO 17633-A-T 19 9 L R M21/C1