HYUNDAI – S-8016.B6

HYUNDAI – S-8016.B6

Stick electrodes for heat resistant applications

Ø 3.2 mm x 350 mm

 

Classifications

AWS A5.5/ASME SFA5.5 E8016-B6

EN 1599 – ECrMo5 B 1 2